2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan

Short Description:


Product Detail

Related Video

Feedback (2)

Persisting in "High quality, Prompt Delivery, Competitive Price", we have established long-term cooperation with clients from both overseas and domestically and get new and old clients' high comments for Global Pvb Film Market, 3m Car Glass Film, Laminated Glass Pvb Interlayer, We've been honest and open up. We glance ahead on your pay a visit to and developing trustworthy and long-term standing relationship.
2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan Detail:

Medium Brown Pvb

Baizan color pvb film for architectural laminated glass.
Baizan can provides plenty of color film for customers choose with stable and accurate color.
production volume >12000t per year
Color pvb MOQ>5000 sq.m.
Payment term:TT LC DP
Delivery time :5-15days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Raw material inspection
In order to ensure the quality of products, we carry out strict inspection on raw materials, according to China national standards。
Detection of PVB resin powder

project volatile viscosity(20℃ 10%/S) Packing density(g/㎝3) Melt index(120℃  21.6kg g/10min) The fog degree(%) Light transmittance(%) Acid value(mgKOH/g) The hydroxyl content(Wt%) Butyl group content(Wt%) transparency

1.Sampling: after every lot of raw material arrive at factory, about 5kg samples will be taken from each lot.
2.Appearance test: white, fine and even, free from any impurity, free- flowing powder or particle.
3.Whiteness: take 2kg of the sample, add 1kg of plasticizer, mix well, extrude and shape the membrane, compare the color
4.The volatility:Weigh up the sample with an analytical balance and place it in a weighing bottle. Keep the bottle in the oven for 3 hours, with temperature 60℃(±1℃) . After taking it out, place it in the dryer for 20-30 minutes and then weigh it.
5.Viscosity:Add resin powder into a paper funnel, put a condensing tube in the 65℃ water bath for 1h, and when it is taken out and cooled to a constant temperature of 20℃±1, pour the sample into a scale cup, and record the time the first drop of solution reach to 50ml, which is the viscosity of the sample
6.Melt index:Weigh the powder and the plasticizer (1:3), adding the plasticizer first and the powder later. After adding it into the melting index flow rate meter, preheat for 4 minutes, add 21.6g weight and start extruding. After 3 minutes, cut off the first section, and then wait for 5 minutes before cutting the second section. The total weight of two sections will be the melting index value.

Customer usage scenarios

awf


Product detail pictures:

2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan detail pictures


Related Product Guide:

Our merchandise are broadly identified and trusted by end users and can satisfy continually developing economic and social requires for 2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan , The product will supply to all over the world, such as: Guinea, Italy, Houston, We integrate all our advantages to continuously innovate, improve and optimize our industrial structure and product performance. We will always believe in and work on it. Welcome to join us to promote green light, together we will make a better Future!
  • In general, we are satisfied with all aspects, cheap, high-quality, fast delivery and good procuct style, we will have follow-up cooperation!
    5 Stars By Elma from Buenos Aires - 2017.03.28 12:22
    This enterprise in the industry is strong and competitive, advancing with the times and develop sustainable, we are very pleased to have a opportunity to cooperate!
    5 Stars By Rachel from Swaziland - 2018.12.25 12:43
    Write your message here and send it to us