With reliable good quality system, great standing and perfect consumer support, the series of products and solutions produced by our organization are exported to quite a few countries and regions for Laminated Pvb Glass, Glass Safety Film For Greenhouses, Window Film For Safety Glass, To acquire a consistent, profitable, and constant growth by getting a competitive advantage, and by continuously increasing the value added to our shareholders and our employee.
Factory wholesale Polyvinyl Butyral Properties - Dark green on light green FG101 – Baizan Detail:

Green on clear C102

Baizan 0.45mm pvb film dark green on light green for car glass
Product volume>12000t per year
Payment terms:TT LC DP
Delivery time:5-10days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Head model impact test
Prepare six glass sheets with a size of 1100mm*500. The composite sheet was placed in 20±5℃ for 4 hours, then remove them in a designated position. Then the head model with a weight of 10kg±0.2g was vertically detached from the sample at a height of 1.5m. The test drop point should be located within a range of 40mm from the sample center. The middle layer is allowed to break, but the human head model cannot penetrate the sample without large debris stripping. Finally, if 4 samples or less than 4 samples meet the above requirements, they will be disqualified. If 5 samples meet the above requirements, 6 new samples will be added. If all 6 samples meet the above requirements, they will be qualified.

ttgtdgsdg

Heat resistance test
Turn on the drying oven and adjust the temperature to 100℃. Prepare a piece of glass with thickness 2 mm.
Put the glass sheets into a 100℃ constant temperature drying oven for 2 hours, then take them out and observe whether there are bubbles or white. Other defects such as bubbles and discoloration shall not occur on the part 15mm beyond the edge or 10mm beyond the crack

Moisture test
Instrument: Moisture meter.
Cut the sample 5g±0.005g and put into the metal plate of the tester. After the machine finish the determination, the moisture value is read

xvcvsdsd


Product detail pictures:

Factory wholesale Polyvinyl Butyral Properties - Dark green on light green FG101 – Baizan detail pictures


Related Product Guide:

Our organization insists all along the quality policy of "product quality is base of business survival; purchaser gratification is the staring point and ending of an business; persistent improvement is eternal pursuit of staff" as well as the consistent purpose of "reputation 1st, purchaser first" for Factory wholesale Polyvinyl Butyral Properties - Dark green on light green FG101 – Baizan , The product will supply to all over the world, such as: UAE, Malaysia, Norway, As operation principle is "be market-oriented , good faith as principle, win-win as objective", holding on "customer first, quality assurance, service first" as our purpose, dedicated to provide the original quality, create excellence service , we won the praise and trust in the industry of auto parts. In the future, We will provide quality product and excellent service in return to our customers , welcome any suggestions and feedback from all over the world.
  • Staff is skilled, well-equipped, process is specification, products meet the requirements and delivery is guaranteed, a best partner!
    5 Stars By Kama from Macedonia - 2017.10.27 12:12
    The factory workers have a good team spirit, so we received high quality products fast, in addition, the price is also appropriate, this is a very good and reliable Chinese manufacturers.
    5 Stars By Pearl from Kenya - 2018.09.29 17:23
    Write your message here and send it to us