Our firm has been concentrating on brand strategy. Customers' satisfaction is our best advertising. We also offer OEM provider for Pvb, Automobile Pvb Film, Pvb Film Thickness, Base within the small business concept of Top quality initially, we want to fulfill more and additional friends within the word and we hope provide the ideal solution and services to you.
Good Quality N-UV lonoplast pvb – N-UV PVB – Baizan Detail:

N-UV PVB

N-UV pvb film is a new interlayer technology for durable architectural safety glass with unsurpassed transmission of natural UV light into spaces appling to special light-requiring flora and fauna
Drop ball impact peel performance
Prepare 6 pieces of 300*300mm glass with 2mm thickness and put them flat, then put the sample on , and then cut it, pay attention to avoid stretching to prevent deformation, and to ensure that the membrane margin outside the glass is about 2mm. Then, the finished mesofilm glass was put into a 160±5℃ vacuum chamber for vacuuming and kept for 90 minutes under a negative pressure of 8.5×104Pa.
Put these 6 samples at a temperature close to 20 + 5℃ for at least 4 hours, respectively, will close on fixed glass bracket of impact test, then the weight is 1040 g + 10 g, steel ball according to the height of about 63.5 mm in diameter from 1200 mm and 1500 mm, 1900 mm and 2400 mm, 3000 mm and 3800 mm in the order hoisting height vertical shock, impact point should be located in the heart of the sample, 25 mm range, the status of each shock after the destruction of the glass

Knock test
Prepare 2 pieces of 76*300mm white glass with thickness of 2mm .Lay the glass flat, put a layer of sample and then a layer of glass, finally cut it down. Pay attention to avoid stretching the film to prevent deformation during cutting, and ensure that the diaphragm margin outside the glass is about 2mm.The finished mesofilm glass was put into a vacuum chamber at 180±5℃ for vacuuming, and kept under a negative pressure of 8.5×104Pa for 30 minutes before being removed.Cool the sheets for half an hour and then place them in an environment of -18℃ (±1℃) for 2 hours. Then remove them and immediately start tapping with a flat hammer from the bottom of the glass
The striking area should exceed at least 1/2 of the glass, then visually observe the degree of falling off of the glass in the striking area, and estimate the percentage of falling off area to determine the corresponding level


Product detail pictures:

Good Quality N-UV lonoplast pvb – N-UV PVB – Baizan detail pictures


Related Product Guide:

We have our own product sales staff, style crew, technical group, QC staff and package staff. We now have strict high quality management procedures for each approach. Also, all of our workers are experienced in printing subject for Good Quality N-UV lonoplast pvb – N-UV PVB – Baizan , The product will supply to all over the world, such as: Uruguay, Cairo, Eindhoven, We aspire to meet the demands of our customers globally. Our range of merchandise and services is continuously expanding to meet customers' requirements. We welcome new and old customers from all walks of life to contact us for future business relationships and achieving mutual success!
  • Wide range, good quality, reasonable prices and good service, advanced equipment, excellent talents and continuously strengthened technology forces,a nice business partner.
    5 Stars By Ivy from Porto - 2018.09.23 17:37
    The goods we received and the sample sales staff display to us have the same quality, it is really a creditable manufacturer.
    5 Stars By Victor from Greece - 2018.03.03 13:09
    Write your message here and send it to us